@article{oai:swu.repo.nii.ac.jp:00002492, author = {角田, 由美子 and 岡村, 浩 and Tsunoda, Yumiko and Okamura, Hiroshi}, journal = {昭和女子大学大学院生活機構研究科紀要, Bulletin of the Graduate School of Human Life Sciences, Showa Women's University}, month = {Mar}, note = {Three types of non-chrome-tanned sheep skin leather processed with different fatliquoring agents and one type of chrome-tanned sheep skin leather as a control were used to make dress gloves for comparison of their functional properties. The results indicated only a slight difference between the non-chrome and chrome-tanned leathers in moisture characteristic, warmth keeping property, temperature within the gloves. The tear strength of the non-chrome leather, however was remarkably lower than that of the chrome leather. Handle according to the KES system was also found poorer in the non-chrome leather. In the glove wearing tests, moreover, the non-chrome leather gloves were found to deform more easily. We conclude that the improvement in tear strength, handle and deformation are required for nonchrome leather to be extensively industrialized., 10, KJ00004724518, 論文, Article}, pages = {85--94}, title = {非クロム羊革を使用したドレス手袋の機能特性}, volume = {15}, year = {2006}, yomi = {ツノダ, ユミコ and オカムラ, ヒロシ} }