Item type |
[ELS]紀要論文 / Departmental Bulletin Paper(1) |
公開日 |
2017-02-16 |
タイトル |
|
|
タイトル |
染色したセルロース繊維の光劣化について |
タイトル |
|
|
言語 |
en |
|
タイトル |
Photodegradation of Cotton, Linen and Rayon Fabrics Dyed with Reactive Dyes |
言語 |
|
|
言語 |
jpn |
キーワード |
|
|
主題Scheme |
Other |
|
主題 |
光劣化 |
キーワード |
|
|
主題Scheme |
Other |
|
主題 |
綿 |
キーワード |
|
|
主題Scheme |
Other |
|
主題 |
麻 |
キーワード |
|
|
主題Scheme |
Other |
|
主題 |
レーヨン |
キーワード |
|
|
主題Scheme |
Other |
|
主題 |
反応染料 |
キーワード |
|
|
言語 |
en |
|
主題Scheme |
Other |
|
主題 |
photodegradation |
キーワード |
|
|
言語 |
en |
|
主題Scheme |
Other |
|
主題 |
cotton |
キーワード |
|
|
言語 |
en |
|
主題Scheme |
Other |
|
主題 |
linen |
キーワード |
|
|
言語 |
en |
|
主題Scheme |
Other |
|
主題 |
rayon |
キーワード |
|
|
言語 |
en |
|
主題Scheme |
Other |
|
主題 |
reactive dyes |
資源タイプ |
|
|
資源タイプ識別子 |
http://purl.org/coar/resource_type/c_6501 |
|
資源タイプ |
departmental bulletin paper |
雑誌書誌ID |
|
|
収録物識別子タイプ |
NCID |
|
収録物識別子 |
AN00038441 |
著者 |
金井, まゆみ
有末, 紘子
小原, 奈津子
KANEI, Mayumi
ARISUE, Hiroko
KOHARA, Natsuko
|
著者所属(日) |
|
|
|
昭和女子大学生活科学部生活環境学科 |
著者所属(日) |
|
|
|
昭和女子大学人間社会学部現代教養学科 |
著者所属(日) |
|
|
|
昭和女子大学人間社会学部現代教養学科 |
記事種別(日) |
|
|
内容記述タイプ |
Other |
|
内容記述 |
論文 |
記事種別(英) |
|
|
内容記述タイプ |
Other |
|
内容記述 |
Article |
抄録(英) |
|
|
内容記述タイプ |
Other |
|
内容記述 |
The influence of reactive dyes on the photodegradation rates of cellulosic fabrics (cotton, linen, rayon) were evaluated. Cellulosic fabrics were dyed with reactive dyes and then exposed to xenon arc lamp light for incremental doses for up to 40 days. Changes in color, tensile strength, a degree of polymerization (D.P.) and cellulose crystallinities were evaluated. After exposure each undyed cellulosic fabric showed a greater loss in tensile strength and D.P. than the dyed fabrics. Tensile strength and D.P. of dyed rayon fabrics decreased at a constant rate. The tensile strength of dyed cotton and linen also decreased similar to that of the dyed rayon, but D.P. of cotton and linen didn't decrease severely as the tensile strength. This suggests that cleavages of glycoside linkage as well as pyranose ring and/or hydrogen bonds may occur by exposure to the light. Crystallinity did not change after the exposure. From this result, it was thought that both crystalline and amorphous regions in the fibers degraded. |
書誌情報 |
學苑
en : GAKUEN
巻 796,
p. 1-7,
発行日 2007-02-01
|
表示順 |
|
|
内容記述タイプ |
Other |
|
内容記述 |
4 |
アクセション番号 |
|
|
内容記述タイプ |
Other |
|
内容記述 |
KJ00004722742 |
ISSN |
|
|
収録物識別子タイプ |
ISSN |
|
収録物識別子 |
13480103 |